Trigonox® 117 can be used as initiator for the solution (co)polymerization of acrylates and methacrylates in the temperature range of 100-170°C, amongst others for the manufacture of coatings. Trigonox® 117 can also be applied as an initiator for the bulk and suspension (co)polymerization of acrylates and methacrylates.
Active oxygen | ≥ 10.83 % |
Appearance | Clear liquid |
Assay | ≥ 99.0 % |
Color | ≤ 30 Pt-Co |
Inorganic + organic hydrolysable chloride | ≤ 100 mg/kg |
TBHP | ≤ 0.099 % |
Density, 20 °C | 0.800 g/cm³ |
Viscosity, 20 °C | 0.9 mPa.s |
Trigonox® B (Di-tert-butyl peroxide) can be used for the market segments: polymer production, polymer crosslinking and acrylics production with their different applications/functions. For more information please check our website and/or contact us.
Brand:Trigonox®
Chemical family:Organic peroxide
CAS number:75-91-2
Physical form:Liquid
Molecular Weight:90.1
Chemical name:tert-Butyl hydroperoxide, 70% solution in water
Brand:Butanox®
Chemical family:Organic peroxide
CAS number:1338-23-4
Physical form:Liquid
Chemical name:Methyl ethyl ketone peroxide in diisononyl phthalate
Brand:Polylite
Appearance:Light yellow transparent viscous liquid
Acid Value:14-20mgKOH/g
Viscosity,25℃:0.14-0.16Pa.s
Solid Content:52-58%
Gel time:25-38min
Brand:Polylite
Appearance:Light yellow transparent viscous liquid
Acid Value:14-22 mg KOH/g
Viscosity, 25℃:1.6-2.3 Pa.s
Solid Content:70-76 %
Gel Time, 25℃:8.5-10.5 min
Thermal Stability, 80℃:≥24h
Brand:Polylite
Appearance: Semi-solid
Epoxy equivalent (g/eq): 170-190
*Hue(G): 3.0Max.
Flash point (℃): 250↑
Solution viscosity (25℃): H~K
Density (g/cm³ 20℃): 1.18
Brand:Polylite
Appearance: light yellow transparent liquid
Density: 1.06±0.02kg/L
Viscosity: 430±150 cps (LVT#3-60rpm/25℃)
Solid content: 62±1.5%
Gelation time: 15-25 minutes
Trigonox® B is an efficient initiator for the production of Low Density Polyethylene (LDPE). It is used both for tubular and autoclave processes. In most cases a combination with other peroxides is used to ensure a broad reactivity range. Trigonox® B may also be used for the polymerization and copolymerization of styrene in the temperature range of 95-185°C. In practice, combinations of two or more peroxides with diverging activities are used to reduce the residual monomer content in the final polymer and to increase reactor efficiency